Torque vs Preload vs Proof Load on RFQ Drawings
OEM RFQ packages for stainless bolts and screws often mix installation torque, joint preload, and proof load—or paste a single Newton-metre figure into a strength box. That invites wrong property marks, dual quotes, and assembly failures that are not the fastener mill’s fault. This guide helps purchasing and engineering lock torque vs preload vs proof load callouts before you send a drawing to Ruike (Ningbo Hongyuan Precision Hardware Manufacturing Co., Ltd. / HY). It complements—not replaces—the bolt grades OEM buyer guide, the fastener strength guide, and the thread engagement vs grip length article.
Plant context: About Us. Browse related hardware under bolts and screws. General RFQ questions: FAQ.
Define the three terms on one print
Torque is an assembly input—how much turning moment the installer applies at the head or nut. It is a process callout (often with lubricant condition and tool method), not a substitute for naming the alloy or the product standard.
Preload (clamp load / preload force) is the tensile force intended in the fastener after tightening so the joint stays clamped under service loads. Engineering owns the target; purchasing must see whether the print states preload, torque, turn-of-nut, or tensioning method—not a vague “tighten securely.”
Proof load is a standardized tensile load a fastener of a given property class or grade must withstand without permanent set. It is a material / strength attribute of the part, not an installation target and not a synonym for service preload.
On RFQs the collision looks like: “A2-70, torque 25 N·m” with no lube note; “proof load = preload”; or copying carbon-steel property marks onto a stainless BOM. Quote desks then split packages or ask for clarification that belonged on Rev A.
When OEM drawings should call torque
Prefer an explicit torque note when assembly is controlled by wrench or torque tool and the buyer’s process owns friction assumptions. Stainless friction scatters with passivation finish, wax, oil, or anti-seize—so dry vs lubricated must travel with the number.
Drawing notes that reduce resubmits
- State torque with units and lubrication condition (dry / lightly oiled / named anti-seize) or point to the buyer’s assembly specification.
- Say whether the figure is head-side or nut-side if the joint uses different finishes.
- Keep tool method (hand torque, click wrench, angle after snug) on the assembly note—not only on a shop traveler the supplier never sees.
- Do not replace alloy, thread system, or product standard with a torque box.
When OEM drawings should call preload (clamp load)
Prefer a preload callout when joint integrity is specified as clamp force or residual tension—gasketed flanges, vibration-critical stacks, or tensioned structural joints—and torque is only a means to that end. If both torque and preload appear, lock which one owns acceptance.
Callouts that keep quotes aligned
- Write target preload (or clamp load) with units and drawing Rev—not only “preload OK.”
- If turn-of-nut or stretch measurement is the method, name that method; do not leave “tighten to preload” without a procedure reference.
- Separate joint design preload from the fastener’s proof-load rating; they answer different questions.
- Washer, coating, and nut finish change friction—list them when torque is used to approximate preload.
When OEM drawings should call proof load / property class
Prefer a proof load or property-class note when the BOM locks strength capability of the fastener itself (for example a buyer-named class under the applicable product standard). Proof load is not an installation torque and must not be pasted into the assembly block.
- Name the standard or drawing Rev that defines the proof load or property mark.
- Keep stainless alloy family (A2/A4 or 304/316-family) on its own line; do not assume carbon-steel grade marks transfer.
- If the print only needs geometry (custom drawing part) without a property class, say so—do not invent a proof-load line for the supplier.
Side-by-side: what belongs on the RFQ package
Use this field set whether you emphasize torque, preload, proof load, or a controlled combination:
- Alloy / material — A2 or A4 (plus 304/316-family note if on the print).
- Thread system — metric or UNC/UNF; keep consistent with the rest of the BOM.
- Standard or drawing — ISO/DIN/ASME callout or drawing Rev + critical dims.
- Property / proof load — only as buyer-named class or standard table; not a DIY Newton figure in the torque box.
- Preload / clamp — target joint tension when engineering owns it; method reference if not torque-only.
- Torque — value + units + lubricant/finish condition when assembly is torque-controlled.
- Head / drive / nut — style and mating hardware that change friction and tool access.
- Surface process — passivation / other finish only if print-required (see passivation vs electropolish).
- Qty + ship window — annual/batch and buyer-stated target date (no invented MOQ or factory lead-time marketing).
Common RFQ mistakes that trigger dual quotes
- Torque number with no dry/lubricated note on stainless.
- Using “proof load” as a synonym for installation preload.
- Carbon-steel property marks pasted onto an A2/A4 line without a buyer standard.
- Preload target with no method (torque vs angle vs tensioner).
- Missing drawing Rev so vendors quote different assembly notes from memory.
Soft CTA: drawing review before you freeze the BOM
Ruike quotes named alloy, geometry, and strength/assembly callouts after manufacturability review. If your print still says only “torque OK / high strength,” send the PDF/STEP for a short drawing review so the quote package locks torque, preload, and proof-load intent. Typical drawing reviews aim for a clear quote path within about 12 hours of a complete package (buyer-stated; not a contractual SLA).
Submit at Get a Quote or Contact. Related reading: bolt grades, fastener strength, engagement vs grip, hex bolts OEM guide, and the site FAQ.
Frequently asked questions — torque, preload, and proof load on RFQ drawings
Is a torque value alone enough for a stainless bolted-joint RFQ?
Usually no. Torque is an assembly input; preload is the clamp force the joint needs; proof load is a material/strength property of the fastener. OEM buyers should name which of these the print owns, plus alloy, standard or drawing Rev, and quantity. A lone “torque to X” note without lubrication, tool, or strength-class context invites dual quotes.
What is the difference between proof load and preload on RFQ drawings?
Proof load is a standardized tensile load the fastener must withstand without permanent set (property of the part/grade). Preload (clamp load) is the tension intended in the assembled joint. Do not paste a proof-load number into a torque box, and do not treat proof load as an installation target unless the buyer’s standard says so.
Should OEM drawings specify dry vs lubricated torque for stainless fasteners?
Yes when torque is a controlled assembly callout. Stainless friction scatters widely with finish, wax, oil, or anti-seize. State lubricant condition (dry / lightly oiled / named anti-seize) with the torque figure, or point to the buyer’s assembly spec. Missing lube notes are a common reason suppliers quote “torque TBD.”
Can proof load replace naming A2/A4 or the strength class?
No. Proof load and property marks sit on top of a named material family and product standard. Keep alloy (A2/A4 or 304/316-family) and any buyer-named strength class or standard on their own lines. Torque/preload notes do not substitute for material locks.
What should I attach so Ruike can quote torque/preload-sensitive parts cleanly?
Send PDF/STEP or approved sample path, alloy and thread system, any buyer torque/preload/proof-load notes (with lube condition if torque is controlled), head/drive geometry, surface process if print-required, annual/batch qty, and target ship window as buyer-stated. Use Get a Quote for drawing review—Ruike does not invent ISO certs, MOQ, or lead times on your behalf.