A Dacromet coating enquiry should identify the exact coating system and governing specification before the process is agreed. This overview explains the stages to discuss with the coating supplier; it is not a bath recipe or operating instruction. For finish selection, use the fastener surface treatment guide.
The specific process flow of Dacromet coating technology is as follows:
Degreasing:
Workpieces with grease must be degreased to ensure coating adhesion and corrosion resistance. There are generally three degreasing methods: organic solvent degreasing, water-based degreasing agent degreasing, and high-temperature carbonization degreasing.
Rust and Deburring:
Workpieces with rust or burrs must undergo a rust and burr removal process. This process is best done mechanically to avoid acid pickling, which can cause hydrogen embrittlement and affect the corrosion resistance of the Dacromet coating.
Coating:
After degreasing and rust removal, the cleaned workpiece should be coated as soon as possible using dip coating, spraying, or brushing. During the coating process, the density, pH value, viscosity, Cr content, temperature, and flow conditions of the coating solution directly affect the coating effect and various properties of the coating. Therefore, it is essential to adjust the relationship between temperature, solution parameters, and centrifuge speed during dip coating.
Pre-baking:
Use the drying or pre-baking step required by the exact coating product and approved process. The supplier must establish its operating window and records; a general blog cannot provide a universal temperature or duration for every coating and part geometry.
Curing: confirm the coating-specific requirements
Agree the curing requirements with the coating supplier for the named coating system. Record how the required part condition is verified rather than assuming that a nominal oven setting proves compliance. Do not transfer a temperature, hold time or chemical mechanism from another coating product without its technical specification.
Cooling:
After sintering, the workpiece must be thoroughly cooled by a cooling system before subsequent processing or finished product inspection. Uneven cooling or excessively rapid cooling may lead to problems such as coating cracking or peeling.
For some workpieces with special requirements, secondary spraying and baking may be necessary to increase the coating thickness and further improve corrosion resistance.
What buyers should confirm
- Exact coating designation and applicable drawing revision.
- Required coverage of threads, holes and recessed areas.
- Agreed coating verification and acceptance records.
- Approved application and curing process for the specified product.